Stainless Steel Jobwork

Property Specification
Material Type Stainless Steel
Grade 304, 316, 410, 430 (varies by requirement)
Density 7.85 g/cm³
Tensile Strength 520 – 1100 MPa
Yield Strength 215 – 510 MPa
Elongation 40% – 60%
Hardness 150 – 220 HB
Modulus of Elasticity 193 GPa
Poisson’s Ratio 0.27 – 0.30
Thermal Conductivity 15 W/m·K
Melting Point 1375 – 1530°C
Corrosion Resistance Excellent in most environments
Magnetic Properties Non-magnetic (except for martensitic grades)
Formability Good (varies with grade)
Weldability Excellent (varies with grade)
Applications Kitchenware, medical equipment, structures
Surface Finish Polished, Matte, or Brushed